item  | Test Method  | The represent value   | |||
Thickness(micro)  | ASTM-D374  | 12 micro   | 15 micro   | 19 micro   | 25 micro   | 
Specific Gravity g/cm3  | ASTM-D1505  | 0.92  | 0.92  | 0.92  | 0.92  | 
Contraction rate Lengthwas/horizontal   | ASTM-D2732  | 52/54  | 52/53  | 52/53  | 51/52  | 
Fog Degree %  | ASTM-D1003  | 1.4  | 1.7  | 2.2  | 2.3  | 
Clarity degree %  | ASTM-D2457  | 125  | 125  | 125  | 120  | 
Coefficent of friction  | ASTM-D1894  | 0.23  | 0.21  | 0.21  | 0.21  | 
Unit area m2/kg  | 91  | 72.8  | 57.4  | 43.7  | |
Tensile strength lengthways/Horizontal N/mm2  | ASTM-D883  | 125/120  | 120/125  | 120/110  | 120/110  | 
Elongation rate of breaking % lengthways/horizontal   | ASTM-D884  | 105/100  | 105/100  | 110/105  | 110/120  | 
Tearing-resisting strength(g)  | ASTM-D1992  | 6.2  | 10  | 14.5  | 17  | 
Heat intensity N/mm2  | Int meth  | 40  | 40  | 39  | 39  | 
Property   | Unit  | Value  | |||
DENSITY   | g/cm3  | 0.92  | |||
THICKNESS  | micro   | 12.5  | 15  | 19  | 25  | 
YIELD  | m2/kg  | 88.8  | 72.5  | 57.2  | 43.5  | 
FLAT WIDTH  | m  | 3000  | 2500  | 2100  | 1600  | 
CENTER FOLD  | m  | 1500  | 1250  | 1100  | 800  | 
SEAL STRENGTH  | gr/cm  | 1100  | 1100  | 1280  | 1420  | 
RESISTANCE  | gr  | 4/10  | 6/11  | 8/13  | 12/20  | 
HAZE  | %  | 2  | 2.2  | 3.2  | 4  | 
GLOSS  | PHOTOM  | 125  | |||